SUS φ2.0 / SUS φ2.0 _4
SUS φ2.0 / SUS φ2.0 Maximum setting for both voltage an…
SUS φ2.0 / SUS φ2.0 Maximum setting for both voltage an…
Al t0.15 / Ni t0.1 It was necessary to consider the hea…
K tc φ1.0 / K tc φ1.0 In order to keep the strands para…
Cu Block / K tc φ3.0 It was not possible to weld the th…
Cu t5.0 / T tc R tc φ 0.3 Cut the tip of each wire of t…
Cu φ0.3 / CU φ0.3 Welded at 6.5V 1.6mS. When the pulse …
Fe:Sn t0.5 / Ni-Cr φ 0.3 Welded. Welding strength can b…
Fe t50.0 / Fe t0.01 Welded two locations with different…
Al t1.0 / T tc φ0.1 To see how the thermocouple wires a…
SUS t2.0 / SUS φ0.65 Welding is possible with a voltage…